I was fortunate to have some notes from a lecture on welding by our inspection company Lloyds EMEA
Welding Code Changes by Bob Pennycook
Lloyd’s Register EMEA Welding Code Changes
OVERVIEW:
Replacement of BS EN287-1:2011 Qualification test
of welders -fusion welding -Part 1: Steels by BS EN
ISO 9606-1:2013
Replacement of BS EN 1418 by BS EN ISO 14732
ISO 15608 /TR Material grouping
Draft for public comment revised ISO15614-1
Draft for public comment revised ISO15614-8
Up coming standard reviews
Welding Procedure and Welder Qualification Review
European standards European standards
WPS qualification to BS EN ISO15607 in the EN/ISO series is not contained in a
single document
BS EN ISO 15614 Specification and qualification of welding procedures for metallic materials
Procedure test
Part 1:Arc welding of Steels and nickel alloys
Part 2: Arc welding of aluminium and its alloys
Part 3: Fusion and pressure welding of non-alloyed and low-alloyed cast irons
Part 4: Finishing welding of aluminium castings
Part 5: Arc welding of titanium, zirconium and their alloys
Part 6: Arc and gas welding of copper and its alloys
Part 7: Overlay welding
Part 8: Welding of tubes to tube-plate joints
Part 9: Underwater hyperbaric wet welding
Part 10: Hyperbaric dry welding
Part 11: Electron and laser beam welding
Part 12: Spot, seam and projection welding
Part 13: Resistance butt and flash welding
Welding Procedure and Welder Qualification Review
European standards European standards
BS EN ISO 15612: 2004: Specification and qualification of welding
procedures for metallic materials -Qualification by adoption of a
standard welding procedure
BS EN ISO 15610: 2003 Specification and qualification of welding
procedures for metallic materials -Qualification based on tested
welding consumables
BS EN ISO 15611: 2003: Specification and qualification of welding
procedures for metallic materials -Qualification based on previous
welding experience
Welding Standard Map.pdf
Welding Procedure and Welder Qualification Review
Standards Update Standards Update
Welder qualification in the EN series is not contained in a single
document
BS EN 287-1:2011 Qualification test of welders -fusion welding -Part 1: steels
BS EN ISO 9606-1: 2013: Qualification test of welders -fusion welding steels.
Part 2: Aluminium and Aluminium alloys
Part 3:Copper and Copper alloys
Part 4:Nickle and Nickel alloys
Part 5: Titanium and Titanium alloys
BS EN ISO14732 : 2013 Welding personnel -Approval testing of welding
operators for fusion welding and resistance weld setters for fully mechanised
and automatic welding of metallic materials
Welding Procedure and Welder Qualification Review
Material grouping Material grouping
Materials are grouped together in ISO15608 to reduce the
number of procedures required. Steel Groups are:
Group 1 C-Mn Steels
Group 2 Fine Grain/TMCP Steels
Group 3 QT or PH (except stainless steels)
Group 4 Low Vanadium Cr-Mo Steels
Group 5 Vanadium Free Cr -Mo Steels
Group 6 High Vanadium Cr-Mo Steels
Group 7 Ferritic, Martensitic and PH Stainless
Group 8 Austenitic Stainless
Group 9 Ni Alloy Steel
Group 10 Duplex Stainless
Group 11 Steels as per Group 1 but with a higher carbon content
Welding Procedure and Welder Qualification Review
Background to BS EN ISO9606-1:2013
The new approach taken by this standard
is to adopt a similar methodology to ASME Section IX .We will
highlight these similarities as we come to them.
The 9606 series cover manual welding. Fully Automatic or
mechanised welding is covered by BS EN ISO 14732
Welding Procedure and Welder Qualification Review
Terminology Terminology
ESSENTIAL VARIABLES:
WELDING PROCESS
PRODUCT TYPE (PLATE /PIPE)
TYPE OF WELD (BUTT/FILLET)
FILLER MATERIAL GROUP
WELDING CONSUMABLE
DIMENSIONS ( THICKNESS/DIAMETER)
WELDING POSITION
WELD DETAILS:
Material, gas, flux backing
Consumable inserts
Single sided, both sided welding
Single layer, multi layer
Leftward/rightward welding
Welding Procedure and Welder Qualification Review
Changes in Ranges in approval Changes in Ranges in approval
MAG/MIG : Welder qualified in dip transfer mode
qualifies for Dip ,globular & Spray but not vice versa.
(131,135,138)
Tests on welds in plates now gives approval for fixed
pipes with a diameter
=
500mm for positions in table 9 &
10.
Tests on welds in plates now gives approval for rotating
pipes with a diameter
=
75mm for positions in table 9 &
10. (PA,PB,PC & PD)
Welding Procedure and Welder Qualification Review
Changes in Ranges in approval Changes in Ranges in approval
TYPE OF WELD (BUTT/FILLET)
Addition of Annex C. Qualification of butt and
fillet in one weld. Single bevel butt with a
permanent backing strip. Minimum thickness
10mm.
Welding Procedure and Welder Qualification Review
Changes in Ranges in approval Changes in Ranges in approval
Welding Procedure and Welder Qualification Review
Changes in Ranges in approval Changes in Ranges in approval
11. FILLER MATERIAL GROUP
Qualification is for filler material not parent material group:
FM1: Non Alloy and Fine Grain Steels
eg:E7108 MMA Electrodes
FM2: High Strength Steels
E10045 MMA Electrodes
FM3: Creep Resisting Steels Cr<3.75%
E8018 MMA Electrodes FM4: Creep Resisting Steels :3.75%12% E8015 MMA Electrodes
FM5: Stainless and Heat Resisting Steels E316L MMA Electrodes FM6: Nickel and Nickel Alloys ENiCrFe-2 MMA Electrodes
Parent material can be any suitable material from Group 1 to 11
Welding Procedure and Welder Qualification Review
Changes in Ranges in approval Changes in Ranges in approval
Welding Procedure and Welder Qualification Review
PERIODS OF VALIDITY PERIODS OF VALIDITY
Welding Procedure and Welder Qualification Review
CERTIFICATION CERTIFICATION
The following non essential variables shell be recorded:
Type of current and polarity
Parent material group/sub group
Shielding Gas
Designation
The standard Process Product type Type of weld Filler material group Consumable type
Dimensions : s ( deposited thickness) / t ( material thickness)
Position
Weld details
Welding Procedure and Welder Qualification Review
Standards Update Standards Update
Is BS EN ISO 9606-1:2013 a harmonized standard for PED?
It has a ZA Annex which states once published in the Official Journal of the European Union under that Directive it will have a presumption of conformity.
The CEN website appears to say this has happened but has not yet been published?
Annex I :3.1.2:To carry out these approvals the third party must perform examinations and tests as set out in the appropriate harmonised standards or equivalent examinations and tests or must have them performed.
Welding Procedure and Welder Qualification Review
BS EN ISO 14732 :2013 Welding Personnel-Qualification
Testing of Welding Operators for Mechanised & Automatic Welding
BS EN ISO 14732 :2013 Welding Personnel-Qualification Testing of Welding Operators for Mechanised & Automatic Welding
Much clearer presentation of essentialvariables, Mandatory functional knowledge test
Optional welding technology test
The same revalidation system as BS EN ISO9606-1:2013
Welding Procedure and Welder Qualification Review
Standards Update Standards Update
ISO/DIS15614-1:2013 SPECIFICATION & QUALIFICATION OF WELDING PROCEDURES FOR METALLIC MATERIALSWELDING PROCEDURE TEST
Proposed to have two levels
Level 1 : Based on ASME Section IX
Level 2: Based on current BS EN ISO15614-1 Welding Procedure and Welder Qualification Review
Standards Update Standards Update
Procedure Tests to Level 2 qualify Level 1 Requirements but not vice-versa
If impact testing, hardness testing or NDE is required by an application standard or specification it shall be carried out and assessed to Level 2 unless specified otherwise.
Welding Procedure and Welder Qualification Review
Standards Update Standards Update
ISO 15608 /TR : 2013
Under review, classification of Group 1 & 11 steels.
BS EN ISO 5817:2014. Revised to include Annex C to cover fatigue loading conditions
BS EN ISO9606 Parts 2 to 5 are coming up for review, it is anticipated that the format will follow that in BS EN ISO9606-1:2013 Welding Procedure and Welder Qualification Review
Get Involved:
http://drafts.bsigroup.com/
Welding Procedure and Welder Qualification Review
Welding Procedures
BSI DRAFT STANDARDS
Welding Procedures
BSI DRAFT STANDARDS
Any questions Any questions
Welding Procedure and Welder Qualification Review
How Lloyd’s Register can help How Lloyd’s Register can help
Qualified and experienced Professionals in the field
Use of “Expert“ programmes to ensure code compliance (TWI C-Spec)
LR Weld Certification Service: Offers a fixed fee “one stop shop” from
witnessing the welding, collecting the samples, NDE & mechanical testing,
certification and certification management
Welding Procedure and Welder Qualification Review